NSF Product and Service Listings
These NSF Official Listings are current as of Monday, July 22, 2024 at 12:15 a.m. Eastern Time. Please contact NSF to confirm the status of any Listing, report errors, or make suggestions.
Alert: NSF is concerned about fraudulent downloading and manipulation of website text. Always confirm this information by clicking on the below link for the most accurate information: http://info.nsf.org/Certified/PwsComponents/Listings.asp?Company=0E110&Standard=061&
NSF/ANSI/CAN 61
Drinking Water System Components - Health Effects
Drinking Water System Components - Health Effects
NOTE: Unless otherwise indicated for Materials, Certification is only for the Water Contact Material shown in the Listing. Click here for a list of Abbreviations used in these Listings. Click here for the definitions of Water Contact Temperatures denoted in these Listings. Products certified to NSF/ANSI/CAN 61 comply with the health effects criteria in NSF/ANSI/CAN 600.
Crossfield Products Corp. | |
3000 East Harcourt Street | |
Rancho Dominguez, CA 90221 | |
United States | |
310-886-9100 |
Facility : Rancho Dominguez, CA
Protective (Barrier) Materials
Water | Water | |||
Water Contact | Contact | Contact | ||
Trade Designation | Size Restriction | Temp | Material | |
Coatings - Tank[1] |
||||
Dex-O-Tex Cemceil Membrane | >= 100 gal. | CLD 23 | CMNT | |
Miracote MiraFlex Membrane C | >= 100 gal. | CLD 23 | CMNT | |
[1] Colors: Natural, white Number of Coats: 1-3 Maximum Field Use Dry Film Thickness(in mils): 78 mils Recoat Cure Time and Temperature: 2 hours at 70º F Final Cure Time and Temperature: 7 days at 70º F Special Comments: Mix ratio for A:B is 28:72 by weight and 52:48 by volume. Use 15 minute induction time for vertical application. Use of Poly Fabric Reinforcement is recommended over cracks and 90 degree angles and is encapsulated within first coat. Apply tack coat of material before positioning fabric, thoroughly saturate and smooth any wrinkles from fabric, then apply coating to maximum dry film thickness. |
Facility : Roselle Park, NJ
Protective (Barrier) Materials
Water | Water | |||
Water Contact | Contact | Contact | ||
Trade Designation | Size Restriction | Temp | Material | |
Coatings - Tank[1] |
||||
MPC Liquid Catalyst | >= 10,000 gal. | CLD 23 | CMNT | |
MPC Powder | >= 10,000 gal. | CLD 23 | CMNT | |
Miracote Catalyst & Powder | >= 10,000 gal. | CLD 23 | CMNT | |
Multipurpose Protective Coating (MPC): MPC Liquid Catalyst & MPC Powder | >= 10,000 gal. | CLD 23 | CMNT | |
Multipurpose Protective Coating Liquid Catalyst | >= 10,000 gal. | CLD 23 | CMNT | |
Multipurpose Protective Coating Powder | >= 10,000 gal. | CLD 23 | CMNT | |
Resistite Liquid | >= 10,000 gal. | CLD 23 | CMNT | |
Resistite Powder | >= 10,000 gal. | CLD 23 | CMNT | |
Resistite Protective Coating: Resistite Liquid and Resistite Powder | >= 10,000 gal. | CLD 23 | CMNT | |
[1] Number of Coats: 2-3 Maximum Field Use Dry Film Thickness (in mils): 60 Recoat Cure Time and Temperature: 4 hours at 72°F Final Cure Time and Temperature: 24 hours at 72°F Special Comments: Mix ratio for A:B is 110:43 by weight for each coat |